Place of Origin:
China
steel bushing for wheel loader
A hardened steel sleeve bushing is a type of bushing made from hardened steel material to provide increased durability, wear resistance, and load-bearing capabilities. It is commonly used in applications where there is high friction or heavy loads, requiring a robust and long-lasting component.
Here are some key aspects related to hardened steel sleeve bushings:
Material: Hardened steel sleeve bushings are typically made from steel alloys that undergo a hardening process to enhance their mechanical properties. Common steel grades used for hardened bushings include tool steel (e.g., D2, A2), bearing steel (e.g., 52100), or alloy steel (e.g., 4140).
Hardening process: The hardening process involves subjecting the steel material to heat treatment, which usually includes heating it to a specific temperature and rapidly cooling it. This process alters the steel's microstructure, resulting in increased hardness and strength.
Design considerations: When specifying a hardened steel sleeve bushing, important design factors to consider include the inner diameter (ID), outer diameter (OD), length, tolerances, surface finish, and any specific features required for proper installation or integration into the application.
Performance Index
|
|
Data
|
|
Hardness
|
HRC
|
58-62
|
|
Max Load
|
N/mm2
|
250
|
|
Max Linear Velocity
|
m/s
|
0.1
|
|
Max PV Value
|
N/mm2.m/s
|
1.5
|
|
WorkingTemperature Limit
|
℃
|
-100~ +350
|
|
Linear Expension Coefficient
|
10-5/℃
|
1.1
|
Performance Index
|
|
Data
|
|
Hardness
|
HV
|
≥650
|
|
Max Load
|
N/mm2
|
200
|
|
Max Linear Velocity
|
m/s
|
0.1
|
|
Max PV Value
|
N/mm2.m/s
|
1.5
|
|
WorkingTemperature Limit
|
℃
|
-100~ +350
|
|
Linear Expension Coefficient
|
10-5/℃
|
1.1
|
Performance Index
|
|
Data
|
|
Hardness
|
HV
|
≥650
|
|
Max Load
|
N/mm2
|
200
|
|
Max Linear Velocity
|
m/s
|
0.1
|
|
Max PV Value
|
N/mm2.m/s
|
1.5
|
|
WorkingTemperature Limit
|
℃
|
-100~ +350
|
|
Linear Expension Coefficient
|
10-5/℃
|
1.1
|
Material and bushing
characteristics
|
|
value
|
Company
|
value
|
|
Maximum load
|
Mpa
|
100
|
psi
|
145,00
|
|
working temperature
|
℃
|
-40 to 300
|
°F
|
-40 to 572
|
|
Max Linear Velocity
|
m/s
|
0.5
|
fpm
|
100
|
|
Maximum PV Value
|
m/sxMPa
|
1.65
|
pis x fpm
|
48,000
|
|
Minimum hardness of sliding layer
|
HB
|
210
|
HB
|
210
|
|
Minimum hardness of dual parts
|
HRC
|
40
|
HRC
|
40
|
Send your inquiry directly to us